Download pdf

MATERIAL Bow and pin high tensile steel, Grade 6, quenched and tempered
SAFETY FACTOR MBL equals 6 x WLL
STANDARD EN 13889 and meets performance requirements of US Fed Spec. RR-C-271 , Grade A
FINISH Hot dipped galvanised
CERTIFICATION As standard; EC Declaration of Conformity

Upon request; 2.1, 2.2, 3.1, MTCa, CE

Item No.

Wll
t

a
mm
b
mm
c
mm
d
mm
e
mm
f
mm
g
mm
h
mm
i
mm
j
mm
k
mm
kg
pcs
GPS13HT 2 13.5 16 34 13 22 51 32 89 57.5 58 22 0.34
GPS16HT 3.25 16 19 40 16 27 64 43 110 71 75 27 0.63
GPS19HT 4.75 19 22 46 19 31 76 51 129 82 89 32 1.00
GPS22HT 6.5 22 25 52 22 36 83 58 144 93 102 32 1.44
GPS25HT 8.5 25 28 59 25 43 95 68 164 108 118 36 2.21
GPS28HT 9.5 28 32 66 28 47 108 75 185 120 131 41 3.18
GPS32HT 12 32 35 72 32 51 115 83 201 137 147 50 4.32
GPS35HT 13.5 35 38 80 35 57 133 92 227 149 162 50 5.67
GPS38HT 17 38 42 88 38 60 146 99 249 164 175 60 7.36
GPS45HT 25 45 50 103 45 74 178 126 300 192 216 60 12.38